LTS40AZH
Melting point 904 ° C. Hardness (GOST 17711−93) HB 10 -1 = 78−88 MPa.
Armature, bushings, bearings
Classification
| Country | Section | Category |
|---|---|---|
| CIS, Russia, Ukraine | Brass (copper-zinc alloy) | Foundry brass |
Information on suppliers
Physical characteristics
| Temperature, °C | $$\alpha\cdot 10^{6}$$, $$K^{-1}$$ | $$\varkappa$$, $$\frac{W}{m\cdot K}$$ | $$\rho$$, $$\frac{kg}{m^3}$$ | $$R\cdot 10^{-6}$$, $$\Omega\cdot m$$ |
|---|---|---|---|---|
| 20 | 113 | 8500 | 90 | |
| 100 | 21.6 |
Standards
| Standard | Description |
|---|---|
| GOST 17711-93 |
Description of physical characteristics
| Parameter | Units of measurement | Description |
|---|---|---|
| $$\alpha\cdot 10^{6}$$ | $$K^{-1}$$ | Coefficient of thermal (linear) expansion (range 20°C–T) |
| $$\varkappa$$ | $$\frac{W}{m\cdot K}$$ | Coefficient of thermal conductivity (the heat capacity of the material) |
| $$\rho$$ | $$\frac{kg}{m^3}$$ | The density of the material |
| $$R\cdot 10^{-6}$$ | $$\Omega\cdot m$$ | Electrical resistivity |