M-MP
To manufacture hot rolled and cold rolled sheets and hot-rolled bars and forgings intended for further machining.
Classification
| Country | Section | Category |
|---|---|---|
| CIS, Russia, Ukraine | Powder metallurgy | Molybdenum powder material |
Chemical composition
| Standard | Fe, % | Si, % | Mg, % | Ca, % | Ni, % | Al, % | Na, % | O, % | Mo, % | W, % |
|---|---|---|---|---|---|---|---|---|---|---|
| GOST 17431-72 | < 0.014 | < 0.005 | < 0.003 | < 0.007 | < 0.005 | < 0.005 | < 0.015 | < 0.3 | > 99.246 | < 0.4 |
Information on suppliers
Mechanical properties at 20 °C
| Rolling | Standard | Size, mm | Tension | Classifiers | $$\sigma _{U}$$, $$MPa$$ | $$\epsilon_L$$, % | Treatment |
|---|---|---|---|---|---|---|---|
| Sheet hot rolled. Annealed. | GOST 17431-72 | 640–690 | 8–10 | ||||
| The bar is hot rolled. Annealed. | GOST 17432-72 | 590–640 | 15–20 |
Standards
| Standard | Description |
|---|---|
| GOST 17431-72 |
Description of chemical elements
| Element | Units of measurement | Description |
|---|---|---|
| Fe | % | Iron |
| Si | % | Silicon |
| Mg | % | Magnesium |
| Ca | % | Calcium |
| Ni | % | Nickel |
| Al | % | Aluminium |
| Na | % | Sodium |
| O | % | Oxygen |
| Mo | % | Molybdenum |
| W | % | Tungsten |
Description of mechanical properties
| Parameter | Units of measurement | Description |
|---|---|---|
| $$\sigma _{U}$$ | $$MPa$$ | Ultimate tensile strength |
| $$\epsilon_L$$ | % | Elongation at break (longitudinal) |