M001
For the manufacture of wire, contact wires, tires and other electrical products.
Classification
| Country |
Section |
Category |
| CIS, Russia, Ukraine |
Copper, copper alloys |
Copper |
Chemical composition
| Standard |
Fe, % |
Bi, % |
Cu, % |
Sb, % |
Te, % |
Pb, % |
As, % |
S, % |
Ag, % |
O, % |
Se, % |
| GOST Р 53803-2010 |
< 0.001 |
< 0.0002 |
> 99.99 |
< 0.0004 |
< 0.0002 |
< 0.0005 |
< 0.0005 |
< 0.0015 |
< 0.0025 |
< 0.04 |
< 0.0002 |
Information on suppliers
Physical characteristics
| Temperature, °C |
$$\rho$$, $$\frac{kg}{m^3}$$ |
$$R\cdot 10^{-6}$$, $$\Omega\cdot m$$ |
| 20 |
8940 |
17 |
Mechanical properties at 20 °C
| Rolling |
Standard |
Size, mm |
Tension |
Classifiers |
$$\sigma _{U}$$, $$MPa$$ |
d5, % |
Treatment |
| Rod |
GOST Р 53803-2010 |
|
|
|
160 |
35 |
|
Analogues
Standards
Description of chemical elements
| Element |
Units of measurement |
Description |
| Fe |
% |
Iron |
| Bi |
% |
Bismuth |
| Cu |
% |
Copper |
| Sb |
% |
Antimony |
| Te |
% |
Tellurium |
| Pb |
% |
Lead |
| As |
% |
Arsenic |
| S |
% |
Sulfur |
| Ag |
% |
Silver |
| O |
% |
Oxygen |
| Se |
% |
Selenium |
Description of physical characteristics
| Parameter |
Units of measurement |
Description |
| $$\rho$$ |
$$\frac{kg}{m^3}$$ |
The density of the material |
| $$R\cdot 10^{-6}$$ |
$$\Omega\cdot m$$ |
Electrical resistivity |
Description of mechanical properties
| Parameter |
Units of measurement |
Description |
| d5 |
% |
Elongation at break |
| $$\sigma _{U}$$ |
$$MPa$$ |
Ultimate tensile strength |