M00k
As raw materials for the production of cast and deformed semi-finished products from copper and copper alloys.
Classification
| Country | Section | Category |
|---|---|---|
| CIS, Russia, Ukraine | Copper, copper alloys | Copper |
Chemical composition
| Standard | Fe, % | Bi, % | Cu, % | Sb, % | Te, % | Pb, % | As, % | S, % | Ag, % | O, % | Se, % |
|---|---|---|---|---|---|---|---|---|---|---|---|
| GOST 859-2001 | < 0.001 | < 0.0002 | > 99.9835 | < 0.0004 | < 0.0002 | < 0.0005 | < 0.0005 | < 0.0015 | < 0.002 | < 0.01 | < 0.0002 |
Information on suppliers
Analogues
| Germany | USA |
|---|---|
| KE-Cu | Cu Grade 1 |
Standards
| Standard | Description |
|---|---|
| GOST 859-2001 | GOST 859 - 2001 |
| GOST 859-14 | |
| DSTU GOST 859:2003 |