M1or
For the manufacture of wire, contact wires, tires and other electrical products.
Classification
| Country |
Section |
Category |
| CIS, Russia, Ukraine |
Copper, copper alloys |
Copper |
Chemical composition
Information on suppliers
Physical characteristics
| Temperature, °C |
$$\rho$$, $$\frac{kg}{m^3}$$ |
$$R\cdot 10^{-6}$$, $$\Omega\cdot m$$ |
| 20 |
8940 |
17.2 |
Mechanical properties at 20 °C
| Rolling |
Standard |
Size, mm |
Tension |
Classifiers |
$$\sigma _{U}$$, $$MPa$$ |
d5, % |
Treatment |
| Rod |
GOST Р 53803-2010 |
|
|
|
160 |
35 |
|
Analogues
| Germany |
USA |
| Cu-OFE |
BCu-1b |
Standards
Description of chemical elements
| Element |
Units of measurement |
Description |
| Cu+Ag |
% |
Copper+Silver |
| Примеси |
% |
Impurities |
| O |
% |
Oxygen |
Description of physical characteristics
| Parameter |
Units of measurement |
Description |
| $$\rho$$ |
$$\frac{kg}{m^3}$$ |
The density of the material |
| $$R\cdot 10^{-6}$$ |
$$\Omega\cdot m$$ |
Electrical resistivity |
Description of mechanical properties
| Parameter |
Units of measurement |
Description |
| d5 |
% |
Elongation at break |
| $$\sigma _{U}$$ |
$$MPa$$ |
Ultimate tensile strength |