M1rO
Classification
| Country | Section | Category |
|---|---|---|
| CIS, Russia, Ukraine | Corrosion-resistant alloys and steels | Corrosion-resistant heat-resistant steel |
Chemical composition
| Standard | Fe, % | Sn, % | Bi, % | Cu, % | Zn, % | Ni, % | Sb, % | Pb, % | As, % | P, % | S, % | O, % | Примеси, % |
|---|---|---|---|---|---|---|---|---|---|---|---|---|---|
| TU 1844-00195375-005-2002 | < 0.005 | 0.03–0.07 | < 0.001 | > 99.9 | < 0.005 | < 0.002 | < 0.002 | < 0.005 | < 0.002 | 0.002–0.012 | < 0.005 | < 0.01 | < 0.1 |
Note: OT: Bi + Sb + As + Fe + Ni + Pb + S + O + Zn
Note: Cu: Cu + Pb + Sn
Note: Microalloying elements are not indicated
Information on suppliers
Analogues
| Germany | USA |
|---|---|
| SE-Cu | ETP |
Standards
| Standard | Description |
|---|---|
| TU 1844-00195375-005-2002 | |
| TU 1844-106-143-2004 | |
| TU 48-21-59-80 |
Description of chemical elements
| Element | Units of measurement | Description |
|---|---|---|
| Fe | % | Iron |
| Примеси | % | Impurities |
| Sn | % | Tin |
| Bi | % | Bismuth |
| Cu | % | Copper |
| Zn | % | Zinc |
| Ni | % | Nickel |
| Sb | % | Antimony |
| Pb | % | Lead |
| As | % | Arsenic |
| P | % | Phosphorus |
| S | % | Sulfur |
| O | % | Oxygen |