MA2-2
for the manufacture of a cliché in the printing industry
Classification
| Country | Section | Category |
|---|---|---|
| CIS, Russia, Ukraine | Magnesium | Magnesium alloys with special properties |
Chemical composition
| Standard | Mg, % | Mn, % | Zn, % | Al, % |
|---|---|---|---|---|
| 95.95–97.5 | 0.15–0.35 | 0.7–1.2 | 2–2.5 |