MA8B
Classification
| Country |
Section |
Category |
| CIS, Russia, Ukraine |
Corrosion-resistant alloys and steels |
Corrosion-resistant heat-resistant steel |
Chemical composition
| Standard |
Fe, % |
Si, % |
Be, % |
Mg, % |
Mn, % |
Ti, % |
Cu, % |
Zn, % |
Ni, % |
Zr, % |
Al, % |
Cl, % |
Примеси, % |
| GOST 2171-90 |
< 0.005 |
< 0.04 |
0.001–0.002 |
89.871–91.999 |
0.2–0.5 |
< 0.005 |
< 0.01 |
0.3–0.8 |
< 0.001 |
< 0.001 |
7.5–8.7 |
< 0.005 |
< 0.06 |