Brand "A"
Classification
| Country |
Section |
Category |
| CIS, Russia, Ukraine |
Corrosion-resistant alloys and steels |
Corrosion-resistant heat-resistant steel |
Chemical composition
| Standard |
Fe, % |
Sn, % |
Bi, % |
Cu, % |
Zn, % |
Sb, % |
Pb, % |
As, % |
Cd, % |
S, % |
Ag, % |
| GOST Р 57774-17 |
< 0.01 |
> 99.754 |
< 0.03 |
< 0.04 |
< 0.005 |
< 0.04 |
< 0.05 |
< 0.05 |
< 0.001 |
< 0.01 |
< 0.01 |
Information on suppliers
Analogues
| Germany |
USA |
| Sn99.90 |
B 339 Grade "A" |
Standards
Description of chemical elements
| Element |
Units of measurement |
Description |
| Fe |
% |
Iron |
| Sn |
% |
Tin |
| Bi |
% |
Bismuth |
| Cu |
% |
Copper |
| Zn |
% |
Zinc |
| Sb |
% |
Antimony |
| Pb |
% |
Lead |
| As |
% |
Arsenic |
| Cd |
% |
Cadmium |
| S |
% |
Sulfur |
| Ag |
% |
Silver |