MBVP
Classification
| Country |
Section |
Category |
| CIS, Russia, Ukraine |
Corrosion-resistant alloys and steels |
Corrosion-resistant heat-resistant steel |
Chemical composition
| Standard |
Fe, % |
Si, % |
B, % |
Mg, % |
Ca, % |
Ti, % |
Ni, % |
Al, % |
C, % |
O, % |
Mo, % |
| TU 48-19-247-93 |
< 0.01 |
< 0.01 |
0.001–0.01 |
< 0.002 |
< 0.003 |
< 0.07 |
< 0.005 |
< 0.004 |
< 0.005 |
< 0.005 |
99.876–99.999 |