MCHP
Molybdenum MCHP is used: for the manufacture of parts for vacuum devices, electronic products; wires with a diameter of 0.40 to 1.9 mm and forged bars with a diameter of 3.0 to 15.0 mm, obtained by drawing and used for the production of special-purpose products; seamless tube blanks; and thin-walled tubes used in the details of color television picture tubes.
MCHP receive vacuum melting sintered molybdenum bars of the brand MCH using carbon as a deoxidizer.
Classification
| Country | Section | Category |
|---|---|---|
| CIS, Russia, Ukraine | Refractory metals, carbide | Molybdenum |
Chemical composition
| Standard | Mo, % |
|---|---|
| GOST 25442-82 | > 99.98 |
Information on suppliers
Standards
| Standard | Description |
|---|---|
| TU 48-19-247-93 | |
| TU 48-19-250-86 | |
| TU 48-19-251-85 | |
| TU 48-19-272-83 | |
| TU 48-19-472-90 | |
| DSTU У 24.4-33338597-005:2012 |