Mg80
for the production of alloys, magnesium-process desulphurization as a chemical reagent and other uses.
Classification
| Country | Section | Category |
|---|---|---|
| CIS, Russia, Ukraine | Magnesium | Primary magnesium |
Chemical composition
| Standard | Fe, % | Si, % | Mg, % | Mn, % | Cu, % | Ni, % | Al, % | Cl, % |
|---|---|---|---|---|---|---|---|---|
| GOST 804-93 | < 0.05 | < 0.05 | < 99.8 | < 0.05 | < 0.02 | < 0.002 | < 0.05 | < 0.005 |
Information on suppliers
Analogues
| Germany | USA |
|---|---|
| H-Mg99.8 | 9980A |
Standards
| Standard | Description |
|---|---|
| GOST 804-93 | |
| DSTU 2187-93 |