MK
The temperature of the hot processing of semi-finished products 650−900 degrees Celsius.
For electrode resistance spot and seam welding of light alloys, collectors of electric motors
Classification
| Country |
Section |
Category |
| CIS, Russia, Ukraine |
Bronze |
Bronze, heatproof |
Chemical composition
Information on suppliers
Physical characteristics
| Temperature, °C |
$$\rho$$, $$\frac{kg}{m^3}$$ |
$$R\cdot 10^{-6}$$, $$\Omega\cdot m$$ |
| 20 |
8920 |
23.1 |
Mechanical properties at 20 °C
| Rolling |
Standard |
Size, mm |
Tension |
Classifiers |
$$\sigma _{U}$$, $$MPa$$ |
$$\sigma_{Y}$$, $$MPa$$ |
$$\psi$$, % |
Treatment |
| Round |
GOST 614-97 |
|
|
|
420 |
400 |
81 |
|
Standards
Description of chemical elements
| Element |
Units of measurement |
Description |
| Cu |
% |
Copper |
| Cd |
% |
Cadmium |
Description of physical characteristics
| Parameter |
Units of measurement |
Description |
| $$\rho$$ |
$$\frac{kg}{m^3}$$ |
The density of the material |
| $$R\cdot 10^{-6}$$ |
$$\Omega\cdot m$$ |
Electrical resistivity |
Description of mechanical properties
| Parameter |
Units of measurement |
Description |
| $$\sigma_{Y}$$ |
$$MPa$$ |
Yield strength |
| $$\sigma _{U}$$ |
$$MPa$$ |
Ultimate tensile strength |
| $$\psi$$ |
% |
Reduction in cross section on fracture |