ICD
The temperature of the hot processing of semi-finished products 750−950 degrees Celsius.
Annealing temperature of 700 degrees Celsius. Hardness after annealing of 8−18 MPa according to Brinell.
Classification
| Country |
Section |
Category |
| CIS, Russia, Ukraine |
Bronze |
Bronze, heatproof |
Information on suppliers
Physical characteristics
| Temperature, °C |
$$\varkappa$$, $$\frac{W}{m\cdot K}$$ |
$$\rho$$, $$\frac{kg}{m^3}$$ |
$$R\cdot 10^{-6}$$, $$\Omega\cdot m$$ |
| 20 |
197 |
8780 |
34.6 |
Mechanical properties at 20 °C
| Rolling |
Standard |
Size, mm |
Tension |
Classifiers |
$$\sigma _{U}$$, $$MPa$$ |
$$\sigma_{Y}$$, $$MPa$$ |
$$\psi$$, % |
$$KCU\cdot 10^{3}$$, $$\frac{J}{m^2}$$ |
Treatment |
| Round |
GOST 614-97 |
|
|
|
764 |
745 |
22 |
294 |
|
Standards
Description of physical characteristics
| Parameter |
Units of measurement |
Description |
| $$\varkappa$$ |
$$\frac{W}{m\cdot K}$$ |
Coefficient of thermal conductivity (the heat capacity of the material) |
| $$\rho$$ |
$$\frac{kg}{m^3}$$ |
The density of the material |
| $$R\cdot 10^{-6}$$ |
$$\Omega\cdot m$$ |
Electrical resistivity |
Description of mechanical properties
| Parameter |
Units of measurement |
Description |
| $$\sigma_{Y}$$ |
$$MPa$$ |
Yield strength |
| $$\sigma _{U}$$ |
$$MPa$$ |
Ultimate tensile strength |
| $$\psi$$ |
% |
Reduction in cross section on fracture |
| $$KCU\cdot 10^{3}$$ |
$$\frac{J}{m^2}$$ |
Impact toughness |