MKLB-2
Classification
| Country | Section | Category |
|---|---|---|
| CIS, Russia, Ukraine | Corrosion-resistant alloys and steels | Corrosion-resistant heat-resistant steel |
Chemical composition
| Standard | Fe, % | Sn, % | Bi, % | Cu, % | Ni, % | Sb, % | Pb, % | As, % | P, % | S, % | Ag, % | O, % |
|---|---|---|---|---|---|---|---|---|---|---|---|---|
| TU 13614181.001-98 | < 0.001 | < 0.001 | < 0.0005 | > 99.9865 | < 0.001 | < 0.001 | < 0.002 | < 0.001 | < 0.001 | < 0.002 | < 0.002 | < 0.001 |
Note: + Se, Te, Cr, Mn, Cd, Si, Co
Information on suppliers
Standards
| Standard | Description |
|---|---|
| TU 13614181.001-98 |
Description of chemical elements
| Element | Units of measurement | Description |
|---|---|---|
| Fe | % | Iron |
| Sn | % | Tin |
| Bi | % | Bismuth |
| Cu | % | Copper |
| Ni | % | Nickel |
| Sb | % | Antimony |
| Pb | % | Lead |
| As | % | Arsenic |
| P | % | Phosphorus |
| S | % | Sulfur |
| Ag | % | Silver |
| O | % | Oxygen |