ML-MP
Classification
| Country |
Section |
Category |
| CIS, Russia, Ukraine |
Corrosion-resistant alloys and steels |
Corrosion-resistant heat-resistant steel |
Chemical composition
| Standard |
Fe, % |
Si, % |
Mg, % |
Ca, % |
Ni, % |
Al, % |
Na, % |
C, % |
La, % |
Mo, % |
W, % |
Примеси, % |
| TU 14-22-200-2005 |
< 0.01 |
< 0.005 |
< 0.002 |
< 0.004 |
< 0.005 |
< 0.003 |
< 0.003 |
< 0.01 |
0.33–0.47 |
99.425–99.67 |
< 0.013 |
< 0.05 |