ML16vch
for corrosion protection of oil and gas pipelines and other underground metal structures
Classification
| Country | Section | Category |
|---|---|---|
| CIS, Russia, Ukraine | Magnesium | Magnesium alloys with special properties |
Chemical composition
| Standard | Fe, % | Si, % | Mg, % | Mn, % | Cu, % | Zn, % | Ni, % | Al, % |
|---|---|---|---|---|---|---|---|---|
| < 0.003 | < 0.04 | 87.453–90.35 | 0.15–0.5 | < 0.003 | 2–3 | < 0.001 | 7.5–9 |
Information on suppliers
Description of chemical elements
| Element | Units of measurement | Description |
|---|---|---|
| Fe | % | Iron |
| Si | % | Silicon |
| Mg | % | Magnesium |
| Mn | % | Manganese |
| Cu | % | Copper |
| Zn | % | Zinc |
| Ni | % | Nickel |
| Al | % | Aluminium |