Mn80A
Classification
| Country | Section | Category |
|---|---|---|
| CIS, Russia, Ukraine | Corrosion-resistant alloys and steels | Corrosion-resistant heat-resistant steel |
Chemical composition
| Standard | Fe, % | Si, % | Mn, % | Cu, % | Al, % | P, % | C, % | S, % |
|---|---|---|---|---|---|---|---|---|
| TU 14-141-11-92 | 9.34–20 | < 2 | > 80 | < 2 | < 6 | < 0.35 | < 0.3 | < 0.01 |
Information on suppliers
Standards
| Standard | Description |
|---|---|
| TU 14-141-11-92 |
Description of chemical elements
| Element | Units of measurement | Description |
|---|---|---|
| Fe | % | Iron |
| Si | % | Silicon |
| Mn | % | Manganese |
| Cu | % | Copper |
| Al | % | Aluminium |
| P | % | Phosphorus |
| C | % | Carbon |
| S | % | Sulfur |