MZH
Classification
| Country |
Section |
Category |
| CIS, Russia, Ukraine |
Corrosion-resistant alloys and steels |
Corrosion-resistant heat-resistant steel |
Chemical composition
| Standard |
Fe, % |
Si, % |
Sn, % |
Bi, % |
Mn, % |
Co, % |
Cu, % |
Zn, % |
Ni, % |
Sb, % |
Pb, % |
As, % |
P, % |
C, % |
S, % |
Примеси, % |
| GOST 2171-90 |
1–1.4 |
< 0.15 |
< 0.1 |
< 0.002 |
0.3–0.8 |
< 0.5 |
89.248–93.7 |
< 0.5 |
5–6.5 |
< 0.005 |
< 0.005 |
< 0.01 |
< 0.04 |
< 0.03 |
< 0.01 |
< 0.7 |
Information on suppliers
Analogues
| Germany |
USA |
| CuNi5Fe |
SB 111 (C70400) |
Standards
Description of chemical elements
| Element |
Units of measurement |
Description |
| Fe |
% |
Iron |
| Примеси |
% |
Impurities |
| Si |
% |
Silicon |
| Sn |
% |
Tin |
| Bi |
% |
Bismuth |
| Mn |
% |
Manganese |
| Co |
% |
Cobalt |
| Cu |
% |
Copper |
| Zn |
% |
Zinc |
| Ni |
% |
Nickel |
| Sb |
% |
Antimony |
| Pb |
% |
Lead |
| As |
% |
Arsenic |
| P |
% |
Phosphorus |
| C |
% |
Carbon |
| S |
% |
Sulfur |