MZHMts
Classification
| Country | Section | Category |
|---|---|---|
| CIS, Russia, Ukraine | Corrosion-resistant alloys and steels | Corrosion-resistant heat-resistant steel |
Chemical composition
| Standard | Fe, % | Mn, % | Co, % | Cu, % | Zn, % | Ni, % | Pb, % | C, % | S, % |
|---|---|---|---|---|---|---|---|---|---|
| GOST 2171-90 | 1–2 | 0.3–1 | < 0.5 | 85.11–89.7 | < 0.3 | 9–11 | < 0.03 | < 0.03 | < 0.03 |
Note: By agreement, the following are allowed:Si, Mg, As, Bi, P, Sn, Sb
Note: Ni: Ni + Co
Information on suppliers
Analogues
| Germany | USA |
|---|---|
| 2.0872 | Cu90Ni10 |
Standards
| Standard | Description |
|---|---|
| GOST 2171-90 | GOST 2171-90 |
Description of chemical elements
| Element | Units of measurement | Description |
|---|---|---|
| Fe | % | Iron |
| Mn | % | Manganese |
| Co | % | Cobalt |
| Cu | % | Copper |
| Zn | % | Zinc |
| Ni | % | Nickel |
| Pb | % | Lead |
| C | % | Carbon |
| S | % | Sulfur |