MNMts50-10-5
Classification
| Country |
Section |
Category |
| CIS, Russia, Ukraine |
Corrosion-resistant alloys and steels |
Corrosion-resistant heat-resistant steel |
Chemical composition
| Standard |
Fe, % |
Si, % |
Bi, % |
Mn, % |
Cu, % |
Zn, % |
Ni, % |
Sb, % |
Pb, % |
Примеси, % |
| TU 48-21-304-86 |
< 0.6 |
< 0.15 |
< 0.002 |
3.5–4.7 |
50–53 |
29.426–36.7 |
9.8–11.2 |
< 0.002 |
< 0.02 |
< 0.9 |
Information on suppliers
Standards
Description of chemical elements
| Element |
Units of measurement |
Description |
| Fe |
% |
Iron |
| Примеси |
% |
Impurities |
| Si |
% |
Silicon |
| Bi |
% |
Bismuth |
| Mn |
% |
Manganese |
| Cu |
% |
Copper |
| Zn |
% |
Zinc |
| Ni |
% |
Nickel |
| Sb |
% |
Antimony |
| Pb |
% |
Lead |