IIC
for the manufacture of parts, working in conditions of vibration loads
Classification
| Country |
Section |
Category |
| CIS, Russia, Ukraine |
Magnesium |
Magnesium alloys with special properties |
Chemical composition
| Standard |
Fe, % |
Mg, % |
Cu, % |
Zn, % |
Ni, % |
|
0.4–0.7 |
98.2–99.08 |
0.4–0.75 |
0.1–0.3 |
0.02–0.05 |
Information on suppliers
Physical characteristics
| Temperature, °C |
$$E\cdot 10^{9}$$, $$MPa$$ |
$$\alpha\cdot 10^{6}$$, $$K^{-1}$$ |
$$\rho$$, $$\frac{kg}{m^3}$$ |
| 20 |
45.6 |
|
1750 |
| 100 |
|
24.8 |
|
Mechanical properties at 20 °C
| Rolling |
Standard |
Size, mm |
Tension |
Classifiers |
$$\sigma _{U}$$, $$MPa$$ |
$$\sigma_{P}$$, $$MPa$$ |
$$\epsilon_L$$, % |
Treatment |
|
|
|
|
|
170–180 |
60–70 |
15–30 |
|
Description of chemical elements
| Element |
Units of measurement |
Description |
| Fe |
% |
Iron |
| Mg |
% |
Magnesium |
| Cu |
% |
Copper |
| Zn |
% |
Zinc |
| Ni |
% |
Nickel |
Description of physical characteristics
| Parameter |
Units of measurement |
Description |
| $$E\cdot 10^{9}$$ |
$$MPa$$ |
Elastic modulus |
| $$\alpha\cdot 10^{6}$$ |
$$K^{-1}$$ |
Coefficient of thermal (linear) expansion (range 20°C–T) |
| $$\rho$$ |
$$\frac{kg}{m^3}$$ |
The density of the material |
Description of mechanical properties
| Parameter |
Units of measurement |
Description |
| $$\sigma _{U}$$ |
$$MPa$$ |
Ultimate tensile strength |
| $$\sigma_{P}$$ |
$$MPa$$ |
Proportionality limit |
| $$\epsilon_L$$ |
% |
Elongation at break (longitudinal) |