MTsr1N3
for the production of ingots, are used as component of the feedstock in the manufacture of cast and wrought magnesium alloys.
Classification
| Country | Section | Category |
|---|---|---|
| CIS, Russia, Ukraine | Magnesium | Charging magnesium alloys |
Chemical composition
| Standard | Fe, % | Si, % | Be, % | Mg, % | Cu, % | Ni, % | Zr, % | Al, % | Nd, % | Cl, % |
|---|---|---|---|---|---|---|---|---|---|---|
| GOST 2581-78 | < 0.01 | < 0.02 | < 0.001 | 98.845–99.6 | < 0.01 | < 0.004 | 0.4–1.1 | < 0.02 | 2.6–3.2 | < 0.005 |
Information on suppliers
Standards
| Standard | Description |
|---|---|
| GOST 2581-78 |
Description of chemical elements
| Element | Units of measurement | Description |
|---|---|---|
| Fe | % | Iron |
| Si | % | Silicon |
| Be | % | Beryllium |
| Mg | % | Magnesium |
| Cu | % | Copper |
| Ni | % | Nickel |
| Zr | % | Zirconium |
| Al | % | Aluminium |
| Nd | % | Neodymium |
| Cl | % | Chlorine |