H-1
for the production of cathode sheets, strips and plates used in the metallurgical industry for alloying steels, alloys, and other manufacturing industries.
Classification
| Country | Section | Category |
|---|---|---|
| CIS, Russia, Ukraine | Nickel, nickel alloys | Primary nickel |
Chemical composition
| Standard | Fe, % | Si, % | Sn, % | Mg, % | Bi, % | Co, % | Cu, % | Zn, % | Sb, % | Pb, % | As, % | Cd, % | P, % | C, % | S, % | Ni + Co, % |
|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|
| GOST 849-2008 | < 0.02 | < 0.002 | < 0.001 | < 0.001 | < 0.0006 | < 0.1 | < 0.02 | < 0.001 | < 0.001 | < 0.001 | < 0.001 | < 0.001 | < 0.001 | < 0.01 | < 0.001 | < 99.93 |
Information on suppliers
Physical characteristics
| Temperature, °C | $$\rho$$, $$\frac{kg}{m^3}$$ |
|---|---|
| 20 | 8800 |
Standards
| Standard | Description |
|---|---|
| GOST 849-2008 | |
| GOST 15515-16 | |
| GOST 849-97 |
Description of chemical elements
| Element | Units of measurement | Description |
|---|---|---|
| Fe | % | Iron |
| Si | % | Silicon |
| Sn | % | Tin |
| Mg | % | Magnesium |
| Bi | % | Bismuth |
| Co | % | Cobalt |
| Cu | % | Copper |
| Zn | % | Zinc |
| Sb | % | Antimony |
| Pb | % | Lead |
| As | % | Arsenic |
| Cd | % | Cadmium |
| P | % | Phosphorus |
| C | % | Carbon |
| S | % | Sulfur |
| Ni + Co | % | Nickel + Cobalt |
Description of physical characteristics
| Parameter | Units of measurement | Description |
|---|---|---|
| $$\rho$$ | $$\frac{kg}{m^3}$$ | The density of the material |