N35HMV
Classification
| Country | Section | Category |
|---|---|---|
| CIS, Russia, Ukraine | Corrosion-resistant alloys and steels | Corrosion-resistant heat-resistant steel |
Chemical composition
| Standard | Fe, % | Mn, % | Cr, % | Ni, % | C, % | Mo, % | W, % |
|---|---|---|---|---|---|---|---|
| 47.44–52.46 | 0.8–0.9 | 8.5–9.5 | 34.3–35.7 | 1.14–1.26 | 0.8–1.2 | 2–4 |
Information on suppliers
Description of chemical elements
| Element | Units of measurement | Description |
|---|---|---|
| Fe | % | Iron |
| Mn | % | Manganese |
| Cr | % | Chrome |
| Ni | % | Nickel |
| C | % | Carbon |
| Mo | % | Molybdenum |
| W | % | Tungsten |