STAINLESS
Classification
| Country | Section | Category |
|---|---|---|
| CIS, Russia, Ukraine | Corrosion-resistant alloys and steels | Corrosion-resistant heat-resistant steel |
Chemical composition
| Standard | Fe, % | Cr, % |
|---|---|---|
| GOST 31569-12 | > 82 | < 18 |
Note: The chemical composition should provide mechanical properties
Note: Chemical framework
Note: The chemical composition is determined by agreement
Note: Cr + Ni + Mo > 35%
Information on suppliers
Standards
| Standard | Description |
|---|---|
| GOST 31569-12 |
Description of chemical elements
| Element | Units of measurement | Description |
|---|---|---|
| Fe | % | Iron |
| Cr | % | Chrome |