NJ
Classification
| Country | Section | Category |
|---|---|---|
| CIS, Russia, Ukraine | Corrosion-resistant alloys and steels | Corrosion-resistant heat-resistant steel |
Chemical composition
| Standard | Fe, % | Mn, % | Ni, % | Zr, % | Al, % | Примеси, % |
|---|---|---|---|---|---|---|
| TU 48-21-129-72 | 10.5–12.5 | 0.2–0.8 | 85.2–89.2 | < 0.1 | 0.1–0.4 | < 1 |
Information on suppliers
Standards
| Standard | Description |
|---|---|
| TU 48-21-129-72 |
Description of chemical elements
| Element | Units of measurement | Description |
|---|---|---|
| Fe | % | Iron |
| Примеси | % | Impurities |
| Mn | % | Manganese |
| Ni | % | Nickel |
| Zr | % | Zirconium |
| Al | % | Aluminium |