CCM
for the production of wire
Classification
| Country | Section | Category |
|---|---|---|
| CIS, Russia, Ukraine | Nickel, nickel alloys | Nickel alloys |
Chemical composition
| Standard | Si, % | Mn, % | Zr, % | Ni + Co, % |
|---|---|---|---|---|
| TU 48-21 - 256 | 2–4 | 0.2–1 | < 0.1 | 93.9–97.8 |