NM-40A
Classification
| Country |
Section |
Category |
| CIS, Russia, Ukraine |
Corrosion-resistant alloys and steels |
Corrosion-resistant heat-resistant steel |
Chemical composition
| Standard |
Fe, % |
Si, % |
Sn, % |
Mg, % |
Bi, % |
Ti, % |
Cu, % |
Zn, % |
Ni, % |
Sb, % |
Pb, % |
As, % |
P, % |
C, % |
O, % |
ET, % |
| TU 48-21-85-85 |
< 0.05 |
< 0.05 |
< 0.001 |
< 0.01 |
< 0.002 |
0.02–0.07 |
39–41 |
< 0.004 |
58.774–60.98 |
< 0.001 |
< 0.002 |
< 0.001 |
< 0.002 |
< 0.02 |
< 0.003 |
< 0.01 |
Information on suppliers
Standards
Description of chemical elements
| Element |
Units of measurement |
Description |
| ET |
% |
Total other items |
| Fe |
% |
Iron |
| Si |
% |
Silicon |
| Sn |
% |
Tin |
| Mg |
% |
Magnesium |
| Bi |
% |
Bismuth |
| Ti |
% |
Titan |
| Cu |
% |
Copper |
| Zn |
% |
Zinc |
| Ni |
% |
Nickel |
| Sb |
% |
Antimony |
| Pb |
% |
Lead |
| As |
% |
Arsenic |
| P |
% |
Phosphorus |
| C |
% |
Carbon |
| O |
% |
Oxygen |