NP
Classification
| Country | Section | Category |
|---|---|---|
| CIS, Russia, Ukraine | Corrosion-resistant alloys and steels | Corrosion-resistant heat-resistant steel |
Chemical composition
| Standard | Fe, % | Si, % | Sn, % | Mg, % | Bi, % | Mn, % | Cu, % | Zn, % | Ni, % | Sb, % | Pb, % | As, % | Cd, % | P, % | C, % | S, % | Примеси, % |
|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|
| GOST 2171-90 | < 0.04 | < 0.03 | < 0.001 | < 0.01 | < 0.001 | < 0.002 | < 0.015 | < 0.005 | > 99.78 | < 0.001 | < 0.001 | < 0.001 | < 0.001 | < 0.001 | < 0.01 | < 0.001 | < 0.1 |
Note: By agreement: Si < 0.006
Note: Ni: Ni + Co
Information on suppliers
Analogues
| Germany | USA |
|---|---|
| Ni 99,8 | F 1 (N02253) |
Standards
| Standard | Description |
|---|---|
| GOST 2171-90 | GOST 2171-90 |
Description of chemical elements
| Element | Units of measurement | Description |
|---|---|---|
| Fe | % | Iron |
| Примеси | % | Impurities |
| Si | % | Silicon |
| Sn | % | Tin |
| Mg | % | Magnesium |
| Bi | % | Bismuth |
| Mn | % | Manganese |
| Cu | % | Copper |
| Zn | % | Zinc |
| Ni | % | Nickel |
| Sb | % | Antimony |
| Pb | % | Lead |
| As | % | Arsenic |
| Cd | % | Cadmium |
| P | % | Phosphorus |
| C | % | Carbon |
| S | % | Sulfur |