NP2E
for anodes, traverses and other parts of electronic devices; Tape thickness of 0.05−2.0 mm, used in electronics and other industries.
Classification
| Country | Section | Category |
|---|---|---|
| CIS, Russia, Ukraine | Nickel, nickel alloys | Prefabricated Nickel |
Chemical composition
| Standard | Fe, % | Si, % | Sn, % | Mg, % | Bi, % | Mn, % | Co, % | Cu, % | Zn, % | Sb, % | Al, % | Pb, % | As, % | Cd, % | P, % | C, % | S, % | Ni + Co, % |
|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|
| GOST 19241-80 | < 0.1 | < 0.1 | < 0.002 | < 0.1 | < 0.002 | < 0.03 | < 0.15 | < 0.1 | < 0.005 | < 0.002 | < 0.01 | < 0.002 | < 0.002 | < 0.002 | < 0.002 | < 0.1 | < 0.003 | < 99.6 |
Information on suppliers
Mechanical properties at 20 °C
Analogues
| Germany | USA |
|---|---|
| Ni 99,4 NiO | Nickel 220 |
Standards
| Standard | Description |
|---|---|
| GOST 19241-80 | |
| GOST 13548-16 | |
| GOST 19241-16 | |
| GOST 2170-16 | |
| GOST 2179-15 |
Description of chemical elements
| Element | Units of measurement | Description |
|---|---|---|
| Fe | % | Iron |
| Si | % | Silicon |
| Sn | % | Tin |
| Mg | % | Magnesium |
| Bi | % | Bismuth |
| Mn | % | Manganese |
| Co | % | Cobalt |
| Cu | % | Copper |
| Zn | % | Zinc |
| Sb | % | Antimony |
| Al | % | Aluminium |
| Pb | % | Lead |
| As | % | Arsenic |
| Cd | % | Cadmium |
| P | % | Phosphorus |
| C | % | Carbon |
| S | % | Sulfur |
| Ni + Co | % | Nickel + Cobalt |
Description of mechanical properties
| Parameter | Units of measurement | Description |
|---|---|---|
| $$\sigma _{U}$$ | $$MPa$$ | Ultimate tensile strength |
| $$\epsilon_L$$ | % | Elongation at break (longitudinal) |