NP2Ev
Classification
| Country |
Section |
Category |
| CIS, Russia, Ukraine |
Corrosion-resistant alloys and steels |
Corrosion-resistant heat-resistant steel |
Chemical composition
| Standard |
Fe, % |
Si, % |
Sn, % |
Mg, % |
Bi, % |
Mn, % |
Co, % |
Cu, % |
Zn, % |
Ni, % |
Sb, % |
Al, % |
Pb, % |
As, % |
Cd, % |
P, % |
C, % |
S, % |
| GOST 19241-80 |
< 0.1 |
< 0.1 |
< 0.002 |
< 0.1 |
< 0.001 |
< 0.03 |
< 0.15 |
< 0.1 |
< 0.003 |
> 99.296 |
< 0.001 |
< 0.01 |
< 0.001 |
< 0.001 |
< 0.001 |
< 0.001 |
< 0.1 |
< 0.003 |
Information on suppliers
Analogues
| Germany |
USA |
| Ni 99,4 NiO |
Nickel 220 |
Standards
Description of chemical elements
| Element |
Units of measurement |
Description |
| Fe |
% |
Iron |
| Si |
% |
Silicon |
| Sn |
% |
Tin |
| Mg |
% |
Magnesium |
| Bi |
% |
Bismuth |
| Mn |
% |
Manganese |
| Co |
% |
Cobalt |
| Cu |
% |
Copper |
| Zn |
% |
Zinc |
| Ni |
% |
Nickel |
| Sb |
% |
Antimony |
| Al |
% |
Aluminium |
| Pb |
% |
Lead |
| As |
% |
Arsenic |
| Cd |
% |
Cadmium |
| P |
% |
Phosphorus |
| C |
% |
Carbon |
| S |
% |
Sulfur |