NUS-5-VI
Classification
| Country | Section | Category |
|---|---|---|
| CIS, Russia, Ukraine | Corrosion-resistant alloys and steels | Corrosion-resistant heat-resistant steel |
Chemical composition
| Standard | Fe, % | Si, % | B, % | Mn, % | Co, % | Cr, % | Ti, % | Cu, % | Ni, % | V, % | Al, % | P, % | C, % | S, % | Nb, % | La, % | Y, % | W, % |
|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|
| 11–13 | < 0.5 | < 0.009 | < 0.4 | 6–7 | 16–18 | 2.5–3 | < 0.07 | 41.889–51.8 | < 0.02 | 1.3–1.8 | < 0.015 | < 0.05 | < 0.007 | 1.4–1.7 | < 0.02 | < 0.02 | 10–12.5 |