O1pch
for the production of tin canning and cooking chemicals
Classification
| Country |
Section |
Category |
| CIS, Russia, Ukraine |
Tin, lead, babity |
Tin |
Chemical composition
| Standard |
Fe, % |
Sn, % |
Bi, % |
Cu, % |
Zn, % |
Sb, % |
Al, % |
Pb, % |
As, % |
S, % |
Примеси, % |
| GOST 860-75 |
< 0.009 |
< 99.915 |
< 0.01 |
< 0.01 |
< 0.002 |
< 0.015 |
< 0.002 |
< 0.025 |
< 0.01 |
< 0.007 |
< 0.085 |
Information on suppliers
Physical characteristics
| Temperature, °C |
$$E\cdot 10^{9}$$, $$MPa$$ |
$$\alpha\cdot 10^{6}$$, $$K^{-1}$$ |
$$\rho$$, $$\frac{kg}{m^3}$$ |
| 20 |
55 |
|
7300 |
| 100 |
|
2.3 |
|
Mechanical properties at 20 °C
| Rolling |
Standard |
Size, mm |
Tension |
Classifiers |
$$\sigma _{U}$$, $$MPa$$ |
$$\epsilon_L$$, % |
Treatment |
| Alloy cast |
|
|
|
|
19–21 |
45–60 |
|
Brinell hardness number
| Rolling |
Standard |
Classifiers |
Value, HBW |
| Alloy cast |
|
|
49–52 |
Casting and technological parameters
Analogues
Standards
Description of chemical elements
| Element |
Units of measurement |
Description |
| Fe |
% |
Iron |
| Примеси |
% |
Impurities |
| Sn |
% |
Tin |
| Bi |
% |
Bismuth |
| Cu |
% |
Copper |
| Zn |
% |
Zinc |
| Sb |
% |
Antimony |
| Al |
% |
Aluminium |
| Pb |
% |
Lead |
| As |
% |
Arsenic |
| S |
% |
Sulfur |
Description of physical characteristics
| Parameter |
Units of measurement |
Description |
| $$E\cdot 10^{9}$$ |
$$MPa$$ |
Elastic modulus |
| $$\alpha\cdot 10^{6}$$ |
$$K^{-1}$$ |
Coefficient of thermal (linear) expansion (range 20°C–T) |
| $$\rho$$ |
$$\frac{kg}{m^3}$$ |
The density of the material |
Description of mechanical properties
| Parameter |
Units of measurement |
Description |
| $$\sigma _{U}$$ |
$$MPa$$ |
Ultimate tensile strength |
| $$\epsilon_L$$ |
% |
Elongation at break (longitudinal) |
Description of the casting and technological parameters
| Parameter |
Units of measurement |
Description |
| melting point |
°C |
The temperature at which solid crystalline body makes the transition to the liquid state and Vice versa |