O2
for the manufacture of babbitt, alloys, solders, tin powders, tubes, foils, tin plating
Classification
| Country | Section | Category |
|---|---|---|
| CIS, Russia, Ukraine | Tin, lead, babity | Tin |
Chemical composition
| Standard | Fe, % | Sn, % | Bi, % | Cu, % | Zn, % | Sb, % | Al, % | Pb, % | As, % | S, % | Примеси, % |
|---|---|---|---|---|---|---|---|---|---|---|---|
| GOST 860-75 | < 0.02 | < 99.565 | < 0.05 | < 0.03 | < 0.002 | < 0.05 | < 0.002 | < 0.25 | < 0.015 | < 0.016 | < 0.435 |
Note: By agreement: Pb < 3.0
Information on suppliers
Analogues
| Germany | USA |
|---|---|
| Sn99.50 | L13010 |
Standards
| Standard | Description |
|---|---|
| GOST 860-75 |
Description of chemical elements
| Element | Units of measurement | Description |
|---|---|---|
| Fe | % | Iron |
| Примеси | % | Impurities |
| Sn | % | Tin |
| Bi | % | Bismuth |
| Cu | % | Copper |
| Zn | % | Zinc |
| Sb | % | Antimony |
| Al | % | Aluminium |
| Pb | % | Lead |
| As | % | Arsenic |
| S | % | Sulfur |