OCS 3-13-4
Classification
| Country | Section | Category |
|---|---|---|
| CIS, Russia, Ukraine | Bronze | Tin cast bronze |
Chemical composition
| Standard | Fe, % | Si, % | Sn, % | Mg, % | Cu, % | Zn, % | Ni, % | Sb, % | Al, % | Pb, % | As, % | P, % | S, % | Примеси, % |
|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|
| < 0.04 | < 0.05 | 2.1–3.5 | < 0.02 | 71.96–85.9 | 9–16 | < 2 | < 0.05 | < 0.05 | 3–6 | < 0.15 | < 0.1 | < 0.08 | < 1.3 |
Note: Cu: Cu + Ni Si Cu: Cu + Ni Si > 0.02 по требованию Al > 0.02 по требованию По согласованию: Al + Si < 0.02 0.02 upon request Al> 0.02 upon request By agreement: Al + Si <0.02
Information on suppliers
Description of chemical elements
| Element | Units of measurement | Description |
|---|---|---|
| Fe | % | Iron |
| Примеси | % | Impurities |
| Si | % | Silicon |
| Sn | % | Tin |
| Mg | % | Magnesium |
| Cu | % | Copper |
| Zn | % | Zinc |
| Ni | % | Nickel |
| Sb | % | Antimony |
| Al | % | Aluminium |
| Pb | % | Lead |
| As | % | Arsenic |
| P | % | Phosphorus |
| S | % | Sulfur |