OVCH-000
Classification
| Country |
Section |
Category |
| CIS, Russia, Ukraine |
Tin, lead, babity |
Tin |
Chemical composition
| Standard |
Fe, % |
Sn, % |
Bi, % |
Co, % |
Cu, % |
Zn, % |
Ni, % |
Sb, % |
Al, % |
Pb, % |
As, % |
Ga, % |
Ag, % |
Au, % |
In, % |
Примеси, % |
| GOST 860-75 |
< 0.0001 |
> 99.999 |
< 5.0E-6 |
< 1.0E-5 |
< 1.0E-5 |
< 3.0E-5 |
< 1.0E-5 |
< 5.0E-5 |
< 0.0003 |
< 1.0E-5 |
< 0.0001 |
< 5.0E-5 |
< 5.0E-6 |
< 1.0E-5 |
< 1.0E-5 |
< 0.001 |
Information on suppliers
Analogues
| Germany |
USA |
| Sn 99.99 DIN EN 610:1995 |
L13002 UNS |
Standards
Description of chemical elements
| Element |
Units of measurement |
Description |
| Fe |
% |
Iron |
| Примеси |
% |
Impurities |
| Sn |
% |
Tin |
| Bi |
% |
Bismuth |
| Co |
% |
Cobalt |
| Cu |
% |
Copper |
| Zn |
% |
Zinc |
| Ni |
% |
Nickel |
| Sb |
% |
Antimony |
| Al |
% |
Aluminium |
| Pb |
% |
Lead |
| As |
% |
Arsenic |
| Ga |
% |
Gallium |
| Ag |
% |
Silver |
| Au |
% |
Gold |
| In |
% |
Indium |