OVCH000
for semiconductor technology
Classification
| Country | Section | Category |
|---|---|---|
| CIS, Russia, Ukraine | Tin, lead, babity | Tin |
Chemical composition
| Standard | Fe, % | Sn, % | Bi, % | Co, % | Cu, % | Zn, % | Ni, % | Sb, % | Al, % | Pb, % | As, % | Ag, % |
|---|---|---|---|---|---|---|---|---|---|---|---|---|
| GOST 860-75 | < 0.0001 | > 99.999427 | < 1.0E-6 | < 1.0E-5 | < 1.0E-5 | < 3.0E-5 | < 1.0E-5 | < 1.0E-6 | < 0.0003 | < 1.0E-5 | < 0.0001 | < 1.0E-6 |
Information on suppliers
Standards
| Standard | Description |
|---|---|
| GOST 860-75 |
Description of chemical elements