PA-ZhGrDK6 (ZGr1.5D3)
plain bearings and other parts of friction units of vehicles, machine tools, a variety of machines and mechanisms. For example, the sleeve of the valve, compressor and other domestic refrigerator.
Classification
| Country | Section | Category |
|---|---|---|
| CIS, Russia, Ukraine | Powder metallurgy | Iron base powder. Antifriction materials |
Chemical composition
| Standard | Fe, % | Cu, % | C, % | S, % |
|---|---|---|---|---|
| GOST 26802-86 | 89–95.1 | 2.7–3.5 | 0.6–1.5 | 1.6–6 |
Information on suppliers
Standards
| Standard | Description |
|---|---|
| GOST 26802-86 |
Description of chemical elements
| Element | Units of measurement | Description |
|---|---|---|
| Fe | % | Iron |
| Cu | % | Copper |
| C | % | Carbon |
| S | % | Sulfur |