PA-ZHH18N15KB (H18N15KB)
Armirovochnye sleeve water lifting pumps, bearings, chemical equipment, engines, instruments, etc.
Classification
| Country | Section | Category |
|---|---|---|
| CIS, Russia, Ukraine | Powder metallurgy | Iron base powder. Antifriction materials |
Chemical composition
| Standard | Fe, % | B, % | Cr, % | Ni, % | C, % | S, % | Mo, % |
|---|---|---|---|---|---|---|---|
| GOST 26802-86 | 60.35–70.98 | 0.02–0.15 | 16–20 | 12–16 | 0.5–1.5 | 0.3–1.5 | 0.2–0.5 |