PA-ZhNGr10Tss (MG30ZHN1K)
Mechanical seals Pump units for processing milk, butter and dairy products; bearings bearings washing baths, dyeing and finishing and drying units of the textile industry, etc.
Classification
| Country | Section | Category |
|---|---|---|
| CIS, Russia, Ukraine | Powder metallurgy | Iron base powder. Antifriction materials |
Chemical composition
| Standard | Fe, % | Mn, % | Zn, % | Ni, % | C, % | S, % |
|---|---|---|---|---|---|---|
| GOST 26802-86 | 39.7–52.1 | < 2.2 | < 1.9 | 40–44 | 7.5–11 | 0.4–1.2 |
Information on suppliers
Mechanical properties at 20 °C
| Rolling | Standard | Size, mm | Tension | Classifiers | $$\sigma _{U}$$, $$MPa$$ | $$KCU\cdot 10^{3}$$, $$\frac{J}{m^2}$$ | Treatment |
|---|---|---|---|---|---|---|---|
| Alloy | GOST 26802-86 | 50 | 8 |
Standards
| Standard | Description |
|---|---|
| GOST 26802-86 |
Description of chemical elements
| Element | Units of measurement | Description |
|---|---|---|
| Fe | % | Iron |
| Mn | % | Manganese |
| Zn | % | Zinc |
| Ni | % | Nickel |
| C | % | Carbon |
| S | % | Sulfur |
Description of mechanical properties
| Parameter | Units of measurement | Description |
|---|---|---|
| $$\sigma _{U}$$ | $$MPa$$ | Ultimate tensile strength |
| $$KCU\cdot 10^{3}$$ | $$\frac{J}{m^2}$$ | Impact toughness |