PbSn10Cu2
as the top layer of thin-walled plain bearings
Classification
| Country | Section | Category |
|---|---|---|
| CIS, Russia, Ukraine | Tin, lead, babity | lead babbit |
Chemical composition
| Standard | Sn, % | Cu, % | Pb, % |
|---|---|---|---|
| GOST 1320-74 | 8–12 | 1–2 | 86–91 |
Information on suppliers
Analogues
| Germany |
|---|
| 1.1202 (C52D2) |
Standards
| Standard | Description |
|---|---|
| GOST 1320-74 |
Description of chemical elements
| Element | Units of measurement | Description |
|---|---|---|
| Sn | % | Tin |
| Cu | % | Copper |
| Pb | % | Lead |