PdAP-2 (PdAP-2, PdAP-2)
Chemical composition
Al Aluminum Rest Fe Iron <0.1 Si Silicon <0.1 Mn Manganese 0.01 — 0.20 Cu Copper <0.01 Zn Zinc 0.6 — 1.0 ET Total other items <0.2
For the production of powder intended for the manufacture of alloys, semi-finished products, chemical compounds of palladium, chemicals and other purposes. Technical requirements — according to GOST 5494−95
Classification
| Country | Section | Category |
|---|---|---|
| CIS, Russia, Ukraine | Precious metals | Palladium, palladium alloys |
Chemical composition
| Standard | Fe, % | Si, % | Sn, % | Sb, % | Al, % | Pb, % | Au, % | Pd, % | Примеси, % |
|---|---|---|---|---|---|---|---|---|---|
| GOST 31291 - 2005 | < 0.02 | < 0.01 | < 0.005 | < 0.05 | < 0.005 | < 0.005 | < 0.01 | > 99.9 | < 0.1 |
Note: Pt + Rh + Ru + Ir < 0.050
Information on suppliers
Standards
| Standard | Description |
|---|---|
| GOST 31291 - 2005 |
Description of chemical elements
| Element | Units of measurement | Description |
|---|---|---|
| Fe | % | Iron |
| Примеси | % | Impurities |
| Si | % | Silicon |
| Sn | % | Tin |
| Sb | % | Antimony |
| Al | % | Aluminium |
| Pb | % | Lead |
| Au | % | Gold |
| Pd | % | Palladium |