PDI 82-18 (PDI-18)
Classification
| Country | Section | Category |
|---|---|---|
| CIS, Russia, Ukraine | Precious metals | Palladium, palladium alloys |
Chemical composition
| Standard | Fe, % | Pd, % | Ir, % | Примеси, % |
|---|---|---|---|---|
| GOST 13462-10 | < 0.04 | 81.56–82.5 | 17.5–18.4 | < 0.22 |
Note: Pt + Rh + Au < 0.180
Information on suppliers
Standards
| Standard | Description |
|---|---|
| GOST 13462-10 | GOST 13462-10 |
Description of chemical elements
| Element | Units of measurement | Description |
|---|---|---|
| Fe | % | Iron |
| Примеси | % | Impurities |
| Pd | % | Palladium |
| Ir | % | Iridium |