PDMKr 900-8,5
Classification
| Country | Section | Category |
|---|---|---|
| CIS, Russia, Ukraine | Precious metals | Palladium, palladium alloys |
Chemical composition
| Standard | Fe, % | Si, % | Bi, % | Cu, % | Pb, % | Pd, % |
|---|---|---|---|---|---|---|
| GOST 18390-14 | < 0.05 | > 0.444 | < 0.002 | 8–9 | < 0.004 | 90–90.5 |
Information on suppliers
Standards
| Standard | Description |
|---|---|
| GOST 18390-14 | GOST 18390-14 |
Description of chemical elements
| Element | Units of measurement | Description |
|---|---|---|
| Fe | % | Iron |
| Si | % | Silicon |
| Bi | % | Bismuth |
| Cu | % | Copper |
| Pb | % | Lead |
| Pd | % | Palladium |