PdSrK-35-5 (PDSrK 60-35)
Classification
| Country |
Section |
Category |
| CIS, Russia, Ukraine |
Precious metals |
Palladium, palladium alloys |
Chemical composition
| Standard |
Fe, % |
Bi, % |
Co, % |
Pb, % |
Ag, % |
Pd, % |
Pt + Ir + Rh + Au, % |
| GOST 13462-79 |
< 0.05 |
< 0.002 |
4.5–5.5 |
< 0.003 |
34.4–35.6 |
59.2–60.8 |
< 0.19 |
Information on suppliers
Physical characteristics
| Temperature, °C |
$$\rho$$, $$\frac{kg}{m^3}$$ |
$$R\cdot 10^{-6}$$, $$\Omega\cdot m$$ |
| 20 |
11320 |
370 |
Mechanical properties at 20 °C
| Rolling |
Standard |
Size, mm |
Tension |
Classifiers |
$$\sigma _{U}$$, $$MPa$$ |
Treatment |
| The band is soft. |
GOST 18390-73 |
|
|
|
600–700 |
|
| Wire is hard. |
GOST 18390-73 |
|
|
|
1100–1300 |
|
Standards
Description of chemical elements
| Element |
Units of measurement |
Description |
| Fe |
% |
Iron |
| Bi |
% |
Bismuth |
| Co |
% |
Cobalt |
| Pb |
% |
Lead |
| Ag |
% |
Silver |
| Pd |
% |
Palladium |
| Pt + Ir + Rh + Au |
% |
Platinum + Iridium + Rhodium + Gold |
Description of physical characteristics
| Parameter |
Units of measurement |
Description |
| $$\rho$$ |
$$\frac{kg}{m^3}$$ |
The density of the material |
| $$R\cdot 10^{-6}$$ |
$$\Omega\cdot m$$ |
Electrical resistivity |
Description of mechanical properties
| Parameter |
Units of measurement |
Description |
| $$\sigma _{U}$$ |
$$MPa$$ |
Ultimate tensile strength |