PdSrN500-450 (Pdsph-45-5)
For the manufacture of jewelry
Classification
| Country |
Section |
Category |
| CIS, Russia, Ukraine |
Precious metals |
Palladium jewelry |
Chemical composition
| Standard |
Fe, % |
Bi, % |
Ni, % |
Pb, % |
Ag, % |
Au, % |
Pt, % |
Pd, % |
| GOST 30649-99 |
< 0.05 |
< 0.002 |
3.68–5.34 |
< 0.004 |
44.5–45.5 |
< 0.05 |
< 0.05 |
50–50.5 |
Information on suppliers
Physical characteristics
| Temperature, °C |
$$\rho$$, $$\frac{kg}{m^3}$$ |
| 20 |
11160 |
Casting and technological parameters
| melting point, °C |
| 1200–1210 |
Standards
Description of chemical elements
| Element |
Units of measurement |
Description |
| Fe |
% |
Iron |
| Bi |
% |
Bismuth |
| Ni |
% |
Nickel |
| Pb |
% |
Lead |
| Ag |
% |
Silver |
| Au |
% |
Gold |
| Pt |
% |
Platinum |
| Pd |
% |
Palladium |
Description of physical characteristics
| Parameter |
Units of measurement |
Description |
| $$\rho$$ |
$$\frac{kg}{m^3}$$ |
The density of the material |
Description of the casting and technological parameters
| Parameter |
Units of measurement |
Description |
| melting point |
°C |
The temperature at which solid crystalline body makes the transition to the liquid state and Vice versa |