LP2
phosphorous pig iron for further recast into steel or melting in iron foundries in the production of castings
Classification
| Country | Section | Category |
|---|---|---|
| CIS, Russia, Ukraine | Cast iron | Pig iron |
Chemical composition
| Standard | Fe, % | Si, % | Mn, % | As, % | P, % | S, % |
|---|---|---|---|---|---|---|
| GOST 805-95 | 94.83–99.2 | 0.5–0.9 | < 2 | < 0.2 | 0.3–2 | < 0.07 |
Information on suppliers
Standards
| Standard | Description |
|---|---|
| GOST 805-95 |
Description of chemical elements
| Element | Units of measurement | Description |
|---|---|---|
| Fe | % | Iron |
| Si | % | Silicon |
| Mn | % | Manganese |
| As | % | Arsenic |
| P | % | Phosphorus |
| S | % | Sulfur |