PG-Yu-NH15SR2
Classification
| Country | Section | Category |
|---|---|---|
| CIS, Russia, Ukraine | Powder metallurgy | Iron powder |
Chemical composition
| Standard | Si, % | B, % | Cr, % | Ni, % | Al, % |
|---|---|---|---|---|---|
| 3 | 2 | 15 | 78.8 | 1.2 |
Note: Typical chemical composition