PZHV4
The powder obtained by the method of recovery, for the manufacture of articles by powder metallurgy, welding materials and other purposes. At a pressure of 400 MPa, a density of at least 5.7 g / cm ³. At a pressure of 700 MPa, a density of at least 6.4 g / cm ³ (size class of 160 and 200)
Classification
| Country | Section | Category |
|---|---|---|
| CIS, Russia, Ukraine | Powder metallurgy | Iron powder |
Chemical composition
| Standard | Fe, % | Si, % | Mn, % | P, % | C, % | S, % |
|---|---|---|---|---|---|---|
| GOST 9849-86 | > 99.22 | < 0.15 | < 0.45 | < 0.03 | < 0.12 | < 0.03 |
Information on suppliers
Standards
| Standard | Description |
|---|---|
| GOST 9849-86 |
Description of chemical elements
| Element | Units of measurement | Description |
|---|---|---|
| Fe | % | Iron |
| Si | % | Silicon |
| Mn | % | Manganese |
| P | % | Phosphorus |
| C | % | Carbon |